Cable Paper

Cable Paper

Cable Paper
Description:
Cable Paper is made of two layers of Aramid paper with one layer of Polyimide film, with good dielectric properties, high heat resistance and mechanical strength, and suitable for electric motors as slot, phase, turn-to-turn, liner insulation in H-class Motor.
Main Specification:
Properties
Values
Structure
212
222
232
242
252
262
2 7.5 2
3 7.5 3
Normal thickness(mm)
0.13
0.15
0.18
0.20
0.24
0.25
0.30
0.30
Thickness Tolerance(mm)
+/-10%
Specific Weight(g/m2)
134
169
205
240
280
315
370
390
Specific Weight tolerance
+/-10%
Tensile Strength (N/cm) unfold ≥
MD
95
150
140
170
190
195
260
280
TD
65
85
100
110
130
160
215
240
Breakdown Voltage(KV)(Unfold) ≥
5.0
8.0
10
12
14
15
18
18
Bonding Strength at 25c.
No Delamination
Bonding Strength at 200c 10min
No Delamination, No Blister, No Adhesive Flow
Testing Method
GB/T 5591.2-2002 or IEC 60626-2:1995